Technician Question T7D09
T7D: Using basic test instruments: voltmeter, ammeter, and ohmmeter; Soldering
What is the characteristic appearance of a cold tin-lead solder joint?
- Dark black spots
- A bright or shiny surface
- A rough or lumpy surface (correct answer)
- A greenish tinge
Correct answer: C, A rough or lumpy surface
Explanation
A cold joint forms when the solder never gets hot enough to flow and wet both the wire and the pad. It then freezes in a rough, lumpy or grainy blob instead of a smooth fillet. The connection is mechanically weak and electrically unreliable, so reheat it until the solder flows smoothly.
Why the other answers are wrong
- A, Dark black spots: Dark black spots usually mean overheating or burned flux residue, not solder that never got hot enough to flow.
- B, A bright or shiny surface: A bright, shiny, smoothly flowing surface is the sign of a good tin-lead joint, the opposite of a cold one.
- D, A greenish tinge: A greenish tinge points to copper corrosion or old flux residue over time, not a joint that was heated too little.